Kiran K. Kokate1, Shrikaant Kulkarni2, Subodh E. Bhandarkar3
1Department of CEES, MIT College of Engineering, Pune (M.S.)
2Department of Chemical Engineering, Vishwakarma Institute of Technology, Pune (M.S.)
3Department of Chemistry, G.V.I.S.H, Amravati (M.S.)
*Corresponding Author E-mail: srkulkarni21@gmail.com
ABSTRACT:
Polymer composites are substitutes to a range of products due to their high strength to weight ratio. Polymer composites are the potential candidates in many of the applications in diverse fields like automobile, healthcare, construction, electronics, etc. which is attributed to their thermal, electrical, optical and mechanical properties. Several methods so far have been employed to synthesize polymer composites. Among conductive polymers, PEDOT [poly(3,4-ethylenedioxythiophene)], stands out due to its excellent stability and high light transmissivity. In this paper in-situ emulsion polymerization technique is employed for the synthesis of poly (3,4-ethylenedioxythiophene) (PEDOT) and is used as a matrix and metal oxides namely Zinc oxide (ZnO), magnetic ferric oxide (Fe3O4) and silver vanadium oxide (AgVO3) as a reinforcing material in preparing a composite out of it. Sonochemical synthesis was preferred over conventional bulk heating process. The process was meticulously followed and optimized so as to develop a stable polymer nanocomposite. Synthesis process was investigated based on reaction time, yield and energy efficiency. The PEDOT & its composite with metal oxides was characterized for its properties namely porosity, mechanical strength, surface texture and morphology using Conductivity, UV-visible spectroscopy, XRD, FTIR and SEM, Particle size analysis, Thermogravimetric and magnetic behavior analysis etc. The results of characterization were found to be in tandem obtained using different analytical tools.
KEYWORDS: Polymer composites, PEDOT
Polythiophene and its derivatives have attracted lot much of attention due to their excellent chemical and physical properties1. Among the derivatives of polythiophene, poly(3,4-ethylenedioxythiophene) (PEDOT), is one of the potential conducting polymers because of its low band gap, excellent environmental stability, high electrical conductivity, and transparency in thin oxidized films. Since the advent of PEDOT in 1989, lot much of investigation on PEDOT has been undertaken. Range of applications like solid electrolytic capacitors, anti-electrostatic agents, transparent electrodes in light emitting diodes, and under-layers for the metallization of printed circuit boards have been reported so far. The synthesis of PEDOT by the techniques like electrochemical and chemical oxidative polymerization and organic synthesis of 3,4-ethylenedioxythiophene (EDOT) has also been already carried out2,3,4 with the latter one being most suitable candidate for mass production5. High-concentration emulsion polymerization of ethylenedioxythiophene (EDOT) in presence of sodium salt of 2-naphthalenesulfonic acid (2-NaNS) as dopant and ferrous sulfate as oxidant has been reported as a distinct technique of polythiophene synthesis prescribed by Japanese researchers. The conductivity of PEDOT obtained by this method was 160 S/cm.
3,4-Ethylenedioxythiophene (EDOT) is the most intensively researched monomer in the past decade or so because of high conductivity, and excellent environmental stability of its polymer poly(3,4-ethylenedioxythiophene) (PEDOT)6,7,8. Further, PEDOT and its derivatives have been dragging attention due to their excellent electronic properties as well. Similarly they are also characterized by low energy-gap, low oxidation energies, high electrical conductivity and stability in the oxidized (p-doped) state. These characteristics make p-doped PEDOT films suitable as electrodes and interfacial hole conducting layers in various types of organic electronic devices, e.g. in light emitting diodes, solar cells, and antistatic or electrochromic coatings8,9,10.
Poly(3,4-ethylenedithiathiophene) (PEDOT), as the all-sulfur analog of PEDOT is for the first time reported by Kanatzidis and coworkers in 199511. Much of the research associated with PEDOT has been attributed to its conjugated structures or characteristic functional groups in its structure12-18. The PEDTT and its derivatives hold lot much of promise in applications as electron donor materials in photovoltaic devices12-16, cathode active materials in rechargeable lithium batteries than PEDOT17. EDTT contains sulfur atoms, in place of oxygen atoms in EDOT, does not exactly justify the very distinct properties exhibited by the two monomers e.g. EDTT has a lower oxidation potential as against EDOT, may be due to electron donating mesomeric effects exhibited by sulfur8-19.
Water is a most ideal medium for synthetic chemistry due to its low operational cost, safety, and green nature20-24 but many organic materials are water-insoluble or only sparingly soluble. To overcome the solubility problem in water, synthetic processes employing surfactant-stabilized emulsions and suspensions have been developed. As a conventional synthetic method, electrochemical polymerization of aromatic heterocyclic compounds with concurrent polymer film deposition has played a very important role in polymer science and it has been proved to be an especially effective method for the preparation of high-quality conjugated polymer film. However, still there is a long way to go to reap up its maximum potential as a “green” pathway. Electrochemical transformations of immiscible materials in aqueous electrolytes have been also been investigated25,26,27 Conducting polymers have been widely studied in aqueous media, such as polypyrrole, polyaniline and PEDOT28-31. However, electrochemical polymerization of EDTT was only found to be possible in organic electrolytes32,33 or ionic liquid34. In order to develop new polymerization system and to broaden the application areas of PEDTT, the mild conditions used for electrochemical polymerization in aqueous solution are perfect choice and ideal for incorporation of enzymes, antibodies or even whole living cell. Based on these considerations above, water still seems to be more attractive for the large scale synthesis of PEDTT and their usage in biosensor field than any other solvent from the viewpoint of cost, handling and safety35-39.
Polythiopheneand its derivatives have caught the attention of the research community because of their excellent chemical and physical properties40-45.Among the derivatives of polythiophene, poly (3, 4- ethylene dioxythiophene) (PEDOT), is one of the most attractive and widely investigated conducting polymer because of its low band gap, excellent environmental stability, high electrical conductivity and transparency in thin oxidized films. PEDOT has been extensively investigated by researchers, for the exploration of its interesting physicochemical properties, such as high conductivity, humidity/gas sensing, redox potential, ion-exchange, excellent environmental stability and ease of preparation from common chemicals45-51. However, in order to make PEDOT suitable for various other applications modification of the properties by doping with nanoparticles have been prescribed52-55. Incorporation of nanoparticles (NPs) into polymers has long been established as an effective, controllable and reliable method of tuning and tailoring the mechanical, magnetic, electrical, optical, thermal and other properties of polymers. The so derived composite materials have superior properties, such as magnetism and conductivity. Nano-inorganic particles were usually coated by polymers to prevent agglomeration due to their high surface activity56,57. Among the nanoparticles magnetite (Fe3O4) has attracted a lot of attention because of having wide range of applications such as magnetic storage devices, catalysis, sensors, and high-sensitivity biomolecular magnetic resonance imaging (MRI) for medical diagnosis and therapeutics. Even though magnetite nanoparticles possess excellent physical properties, the nanoparticles alone cannot be used for any of the applications. These applications require the material to be flexible. Therefore, various attempts have been made to synthesize ceramic-polymer nanocomposites. Since the development of magnetic materials, considerable research effort has been made to incorporate magnetic materials into conjugated polymers to develop novel magnetic and electrically conducting organic/inorganic hybrids, which can be further used in electromagnetic interference shielding, information storage, microwave absorbing devices and biomedicine58,59. Han et al reported that Fe3O4/PANI microspheres can be used for the removal of Cr ions. They also studied the magnetic properties and found to possess super paramagnetic behavior even after the preparation of nanocomposite60. Though there are few reports on the synthesis of PANI-magnetite nanocomposites but there are no reports on the PEDOT-magnetite nanocomposites. Lee et al studied the polyaniline–polystyrene sulfonate/Fe3O4 nanoparticles61. They reported that the material exhibited excellent colloidal stability in water and favorable electrical conductivity of approximately 0.08 S cm−1.
Polymer composites have been vigorously developed and extensive utilization of polymer materials has led to the polymer composites62. The intensive use of polymer in broad use has led to the development of materials for specific applications namely composites63 Ceramic materials are typically brittle, possess low dielectric strength and in many cases are difficult to process requiring high temperature. On the other hand, polymers are flexible, can be easily processed at low temperatures and exhibit high dielectric break down fields64 and has wide applications now-a-days in thin film devices65. Recently, high dielectric constant ceramic based polymer nanocomposites have attracted significant interest. These materials generally show relatively low dielectric loss because both the polymer and the ceramic particles are dielectric in nature. So far, many high dielectric constant polymer composites have been prepared by introducing ceramic nanoparticles such as BaTiO366-72 ZrO268,and TiO273-76, The polymer matrices include poly(vinylidene fluoride) [PVDF] and its copolymers, poly(vinylidene fluoride-co-trifluoroethylene) [PVDF–TrFE],[72] poly(vinylidene fluoride-co-hexafluoropropylene) [PVDF–HFP] [166] and poly(vinylidene fluoride-co-trifluoroethylene–chlorotrifluoroethylene) [PVDF–TrFE– CTFE]72,77, polycarbonate (PC)78, epoxy resin79, sulfonate styrene-b- (ethylene-ranbutylene)-b-styrene (S-SEBS), polypropylene (PP)72,79,80, poly(methyl methacrylate) [PMMA]81 and polystyrene (PS)81. Although a wide variety of high dielectric constant polymer/ceramics nanocomposites have been prepared, very little effort has been devoted for preparing composites with the inherent low loss of the base polymer.
Various techniques have been developed to prepare conducting magnetic nanocomposites, including the direct precipitation of iron salt in a solution of conjugated polymer21,22,23.In situ synthesis of conjugated polymer via an oxidative or electrochemical procedure in the presence of well dispersed magnetic nanoparticles and the simultaneous gelation of iron oxide and polymerization of monomer25,26. However, most composite particles that are prepared by these processes typically have a wide size distribution and contain multi-particle aggregates of iron oxide, producing an uncontrolled structure and unpredictable material properties27,28. Therefore, in the present work the Fe3O4/PEDOT nanocomposites were prepared using chemical reduction method. The material was studied for its structural, micro structural, thermal, optical and magnetic properties by using various characterization techniques29,30. Finally, an attempt has also been made to correlate the above properties.
MATERIALS AND METHODS :
PEDOT-ZnOnano-composite:
A. Experimental set up:
Fig.1. shows the characteristic structure of the polymer PEDOT. The conductivity of PEDOT film can be enhanced by adding inorganic compound like ZnO. The additive induces a conformational change in the PEDOT chains. Both coil and linear or expanded-coil conformations exist in untreated PEDOT films, which predominantly contribute to high conductivity of PEDOT films. This conformational change results in an increase in the intra-chain and inter-chain charge-carrier mobility, so that the conductivity is enhanced [4]. Fig.2. shows the spherical micelle formed by the surfactant, Sodium Dodecyl sulfate (SDS) which is a surfactant which provides a template and forms spherical structure (micelle) which in itself acts as a micro-reactor for the polymer to form and thus the concentration of emulsifier influences the size of polymer chain. Fig.3. shows the experimental set up used for the polymerization and composite preparation purpose. For emulsion polymerization of EDOT semi batch reactor equipped with sonication probe (sonotrode), magnetic stirrer and nitrogen supply was used. The reactor provided for continuous monomer supply and introduction of sonotrode through two inlets of a four necked glass reactor. The product (nanocomposite) obtained on completion of the reaction was subjected to centrifugation followed by drying using heater and tray drier.
B. synthesis of PEDOT-ZnOnano-composite:
All the chemicals used for experimentation purpose were AR grade. For in-situ emulsion polymerisation of 3,4-ethylenedioxythiophene (EDOT) semi batch reactor was used. Emulsion polymerization of 3,4-ethylenedioxythiophene (EDOT) was carried out in a 500 ml four necked reaction vessel equipped with sonication probe, thermometer, nitrogen supply and drop wise monomer addition. Pre-weighed sodium lauryl sulphate (surfactant) and 250 ml of water were mixed in a beaker and the solution was subjected to sonication for complete dissolution to take place at room temperature. Then ammonium persulphate as a initiator was added to the reaction mixture with simultaneous stirring at ambient temperature. Further EDOT (monomer) was added at the rate of 1 drop/sec. The reaction mixture was then sonicated for about 2 hrs. at 275 rpm. Nitrogen was continuously bubbled through the solution for providing inert atmosphere to prevent oxygen from reacting with the radicals generated in the reaction which can otherwise hamper the polymerization process. On polymerization of the product PEDOT black in colour was centrifuged with centrifuge REMI, ω = 15000 rpm, washed by acetone (3 X 15 ml), dried by tray drier. The filler, ZnO was added slowly during polymerization of PEDOT with constant stirring using ultrasound. The experimental set up used for the experimentation purpose is as shown in fig.3.
Fig.1 Characteristic structure of the polymer PEDOT
Fig.2 Micelle formation during emulsion polymerization
Fig. 3 Experimental set up for the synthesis of PEDOT-ZnO nanocomposite PEDOT- Fe3O4 nano-composite
A. Synthesis of Fe3O4 Nanoparticles:
The reagents used for chemical synthesis of iron particles were FeCl3⋅6H2O, FeSO4⋅7H2O and NaOH. The wet chemical synthesis involved hydrolysis of Fe3+ and Fe2+ salts in the presence of NaOH. FeCl3 (2M) : FeCl2 (1M) were dissolved in equal volume of distilled water, then stirred for 30 min at room temperature. In the reaction mixture, NaOH was added drop wise and the pH of the solution was adjusted to ~ 11-12. Finally, black precipitate was obtained confirming the formation of Fe3O4.
These particles were then separated out from the solution by using a strong magnet and then were washed many times with distilled water.The precipitated magnetite was black in color .The powder was then dried in hot air oven at 100°C for overnight. The overall reaction can be written as;
Fe2+ + 2Fe3+ + 8OH- → Fe3O4 + 4H2O
B. Synthesis of PEDOT- Fe3O4 Nanocomposite:
The PEDOT layer was prepared by in situ chemical oxidative polymerization. First (0.1, 0.15, 0.2, 0.25 g) of already synthesized Fe3O4 nanoparticles were dispersed in 40 ml of acetonitrile by agitation and ultrasonication followed by transferring it into a flask. Moreover, a given volume of monomer, EDOT (0.0035 M) was added and stirred with reflocculated Fe3O4 for 1 h to ensure complete mixing. Additionally, a given amount of oxidizing agent (2 times of EDOT concentration in terms of molar ratio) FeCl3 (0.007 M) was dispersed in 40 ml of acetonitrile, followed by drop wise addition and the subsequently refluxed at 86 °C for 12 h.
The product obtained was then washed repeatedly with ethanol and deionized water, and the powder was dried at 60 °C for 12 h [31].
RESULTS AND DISCUSSION :
A. PEDOT-ZnO nanocomposite characterization
1. Scanning electron Microscopy (SEM) analysis :
Fig.4 SEM image of PEDOT
Fig. 5 SEM image for PEDOT-ZnO composite
Fig. 4. Shows the SEM-image PEDOT with alamellar or shapeless flat sheet structure, and PEDOT chains lying parallel to one another with doping agent ZnO embedded in the form of inclusion in the PEDOT matrix. The composite is washed with milli Q water to purify it which brings about increase in conductivity from 1 S/cm to approx.150 S/cm. In order to enhance PEDOT conductivity heating of it is proposed which can lead to its post polymerization resulting into comparatively more regular structure. Fig.5. is meant for SEM image of the nanocomposite of PEDOT with ZnO which shows the latter one being distributed in the body of PEDOT in the form of inclusion which add up conductivity to the former one.
2. FTIR analysis:
FT-IR spectrum of synthesized polymer shows the peaks at 1525 and 1330 cm−1 (C-C and/or C=C stretching vibrations in the thiophene ring), 1197 cm−1 (for C-O-C bond), 991, 850 and 690 cm−1 (ν(C-S) and δ(C-H)) [6]. Thus one can conclude that emulsion polymerization product is PEDOT.
3. UV-Visible spectroscopy
Fig. 6 UV spectrum for ZnO NP’s with variation in precursor conc.
Fig. 6 shows the absorption spectrum for the kinetics followed in ZnO nanoparticles synthesis with variation in the concentration of precursor, Zn(NO3)2.6H2O. The sharpness in the SPR is prominent indicating not much increase in size of nanoparticles and further morphology of the NP’s still remain more of a spherical in nature. The kinetics of particles formation was proportional to the effect of reducing agent concentration. Stable, spherical crystalline ZnO NP’s with well defined dimensions (average size of 40 ± 2 nm) were obtained, on treating aqueous Zinc nitrate with the aqueous NaOH solution.
4. Particle size analysis
Fig. 7 Particle siz distribution (PSD) histogram for ZnO NP’s
Fig. 7 shows the histogram of particle size distribution of ZnO nanoparticles. The histogram shows that the nanoparticles are polydispersed and the particle size diameter ranges from 30 to 57 nm and the average particle size diameter comes out to be 40.5 nm which is in harmony with that confirmed from other analytical techniques like UV Spectroscopy, SEM etc.
B. PEDOT- Fe3O4 Nanocomposite characterization
1. XRD analysis
Fig. 8 An overlay of XRD images of PEDOT and PEDOT-Fe3O4 nanocomposite
Fig. 8 Shows that the XRD pattern of pure PEDOT and PEDOT-Fe3O4 nanocomposites. It has been seen that the presence of a broad amorphous peak ~ 25 degree in all the samples confirms the formation of PEDOT as well the presence of PEDOT in all the composites. The rest of XRD peaks were indexed by matching with the standard XRD pattern of Fe3O4 (JCPDS Card No: 88-0315), which further confirms the formation of PEDOT-Fe3O4 nanocomposite. It has been also observed that with the increase in Fe3O4 content the intensity of the magnetite peaks were on the rise whereas the amorphous peak is decreasing, which indicates the increase in crystallinity of the nanocomposites. The average particle size of nanoparticles was estimated based on Debye-Scherrer correlation of particle diameter (D) with peak width at half maximum for Bragg diffraction from ideal single domain crystallites L= kλ/(βcosθ). The average size of the Fe3O4 particles calculated from the Scherrer’s equation was ~ 50 nm.
2. Scanning electron microscopy (SEM) analysis
Fig. 9 SEM images of a) Pure Fe3O4, b) Pure PEDOT nanoparticles, c) 0.1 g, d) 0.15 g, e) 0.2 g, f) 0.25 g of Fe3O4 in PEDOT
Fig.9 depicts the SEM micrographs of the pure Fe3O4, pure PEDOT and PEDOT-Fe3O4 nanocomposites. Figure (a) shows that the shape of the pure Fe3O4 nanoparticles were spherical with particle size in the range of 50-52 nm which were more or less uniformly distributed. The shape of the nanoparticles were almost spherical in nature while very few relatively large particles were oblongated which may be attributed to agglomeration or uneven growth. Fig (b) shows the SEM images of the PEDOT nanoparticles. The morphology of the polymer material shows that the PEDOT nanoparticles formed were of uniform size. From Fig.(c- f), it can be seen that Fe3O4 nanoparticles were uniformly embedded in the polymer matrix. However, it can be clearly seen that the agglomeration of the particle is clearly visible at higher loading percentage of Fe3O4 nanoparticles.
3. Thermogravimetric analysis
Fig. 10 Thermogravimetric analysis curves for pure PEDOT and PEDOT-Fe3O4 nanocomposite
Fig. 10 shows TG curves of the pure PEDOT and PEDOT/Fe3O4 nanocomposites. It can be seen that for pure PEDOT complete degradation of polymer occurs at 650 oC but with the incorporation of magnetite nanoparticle the degradation temperature was found to be shifted towards the higher temperature, which may be due to the higher degradation temperature of the magnetite nanoparticles. Hence, with the incorporation of the magnetite nanoparticles the thermal stability of the material got increased.
4. Particle size analysis
Fig.11 Particle size distribution (PSD) histogram for Fe3O4 NP’s
Fig. 11 shows the histogram of particle size distribution of Fe3O4 nanoparticles. The histogram shows that the nanoparticles were polydispersed and the particle size diameter ranges from 30 to 57 nm and the average particle size diameter comes out to be 48-50 nm which is in harmony with that confirmed from other analytical techniques like UV Spectroscopy, SEM etc.
5. UV-Visible spectroscopy
Fig. 12 UV-Vis spectrum for pure PEDOT and PEDOT-Fe3O4 nanocomposite
Fig. 12 shows the UV-Vis Spectrum of the PEDOT- Fe3O4 nanocomposite. It can be observed that with increase in Fe3O4 content the absorption peak is getting shifted towards the higher wavelength i.e. red shift is observed. This may be due to the fact that with increase in the Fe3O4 content the agglomeration of the particle occurs which in turn decreases the band gap hence absorption peak shifts towards the higher wavelength side.
6. Magnetic behavior analysis:
Fig. 13 Graph of Magnetization V/s magnetic field strength for pure PEDOT and PEDOT-Fe3O4 nanocomposite
Fig. 13 shows the magnetization vs magnetic field loops of the pure PEDOT and PEDOT/Fe3O4 nanocomposites. Development of saturated loop confirms the magnetic nature of the samples. Usually, in case of pure ferromagnetic samples, a remnant magnetization and coercive field is observed but in this case no such behavior is observed. Hence, these samples show super paramagnetic behavior. The saturation magnetization (Ms) is found to be strongly dependent on the amount of Fe3O4 content in the composite. It can be seen that for pure magnetite it is found to be ~ 65 emu/g whereas for the nanocomposite which contains 0.1 g magnetite the value of Ms decreases to ~ 20 emu/g. The reduction in the value of Ms may be due to the nonmagnetic nature of the polymer. However, with further increase in magnetite content the value of Ms increases to ~ 30 emu/g. The increase of Ms Value with the increase in loading percentage of BFO nanoparticles can be explained by the following equation:
Ms= Φms --- ----------- (2)
Where Ms is related to the percentage of BFO nanoparticles and the saturation moment of a single particle (ms). The magnetization measurement indicated that the nanocomposite can be used for information storage applications.
C. PEDOT – SVO nanocomposite characterization
1. UV-Vis spectroscopy
Fig. 14 UV spectrum for the kinetics followed in the SVO nanoparticles formation
Fig. 14 shows the absorption spectrum for the kinetics of silver vanadium oxide SVO nanoparticles synthetic route. The sharpness in the SPR indicates the formation of spherical nanoparticles and more of isotropic and less of anisotropic nanoparticles. There is no Red shift in the Surface Plasmon Resonance (SPR) without peak broadening and decrease in peak width and consequently comparatively more peak sharpness as well as morphology of the NP’s remain more of a spherical in nature. Stable, spherical crystalline SVO NPs with welldefined dimensions were obtained.
2. Particle size analysis:
Fig. 15 Histogram for particle size distribution of SVO nanoparticles
Fig. 15 Shows a histogram for particle size distribution for SVO nanoparticles ranging from 3.5 to 7.5 nm with an average diameter of about 5.5 ppm which further shows that particles are poydispersed but over a very narrow range varying between 3.5 to 7.5 nm.
3. Scanning electron microscopy
Fig. 16 SEM micrograph of the pure SVO
Fig. 16 depicts the SEM micrograph of the pure SVO and it can be clearly seen that the shape of the pure SVO nanoparticles were flat, sheet like which are more or less uniformly distributed throughout surface while very few relatively large particles are observed which may be due to the effect of agglomeration.
D. Characterization for PEDOT-metal oxide nanocomposites in Sensor applications:
In dye-sensitised solar cell (DSSC), The choice of semiconductor is influenced by the conduction band energy and density of states which leads to charge separation and minimization of the recombination. Secondly, the high surface area and morphology of semiconductors is to maximize the light absorption by the dye molecules keeping intact the good electrical connectivity of the substrate. The semiconducting metal oxides such as titania (TiO2), zinc oxide (ZnO), and tin oxide (SnO2) are found to exhibit excellent optical and electronic properties which lead to their use as photoelectrode materials for DSSCs. To enhance the light harvesting efficiency, the metal oxide nanostructures must have a high surface-to-volume ratio for bringing about high absorption of dye molecules. The porous nanocrystalline ZnO films provide the large surface for dye molecule adsorption and therefore, the suitable energy levels at the semiconductor-dye interface allow for the effective injection of electrons from the dye molecules to the semiconductor in DSSC.
When compared with other photovoltaic materials, anatase phase TiO2 has a comparative advantage by virtue of its stability, wide band gap leading to its wide use in the device design. ZnO nanomaterials are better placed than TiO2 photoanodes in respect of wide band gap with higher electronic mobility, which facilitate efficient electron transport, with reduced recombination loss in DSSCs. Earlier studies show the use of ZnO material photoanodes for the application in DSSCs. Although the conversion efficiencies of ZnO (0.4-5.8%) is comparably lower than TiO2 (~11%), ZnO is still a better alternative to TiO2 due to its ease of crystallization and anisotropic growth.
PEDOT-ZnO as Photoanode in DSSC’s:
ZnO nanomaterials so far used in many technological applications as a photocatalyst, photovoltaic material, gas sensor, optical coating, structural ceramic, electrical circuit visitor, biocompatible material, bone implants, and spacer material for magnetic spin valve systems etc. The morphology of ZnO is the crucial characteristic for determining the physical and electrical properties. 1D ZnO nanomaterials like NRs, NWs and NTs possess significant surface areas compared to bulk materials, thereby exhibit unique chemical, physical, optical and the electric properties and reduced recombination rate for the excited electron-hole pair and contribute towards the electrical and photoelectrochemical applications.
The vertically grown ZnO NRs allow shorter and the uninterrupted electrical pathways for the photo generated carriers and improves the charge separation and charge transport properties in many photo electrochemical devices like dye sensitized solar cells (DSSCs). However, it is expected that the highly oriented ZnO NRs could be the potential electrode and photo catalyst material for several photoelectrochemical applications. S. Ameen et al reported the ZnO nanorods (NRs) based photo anode for the fabrication of DSSCs.
Fig. 17 Low and high resolution FESEM images of the ZnO NR thin films obtained with the precursor solutions of ethanol/DI water with ratios of (a, b) 0 : 100 v/v, (c, d) 50 : 50 v/v and (e, f) 80 : 20 v/v.
The morphology of the ZnO NR thin films synthesized by the hydrothermal process with variations in the ethanol/DI water precursor solution is depicted in FESEM images (Fig. 18). with an ethanol/DI water ratio of 0:100 v/v as the precursor solution, the distorted hexagonal TiO2 NRs (Fig. 17 (a, b)) of average particle size ~100-200 nm were obtained. However, the round headed ZnO NRs with ethanol/DI water (50: 50 v/v) as the precursor solution (Fig. 17 (c, d)) was formed. The grown ZnO NRs possess the average diameters of ~50–70 nm respectivelyly. The high amount of ethanol is responsible for achieving the highly ordered nanorods.
Fig. 18 XRD patterns of nanospikes decorated ZnO sheets
XRD patterns of the nano spikes decorated ZnO sheets obtained all the diffraction peaks appeared at 32.3o (100), 35.2o (002), 36.8o (101), 48.2o (102), 57.2o (110), 63.5o (103) and 66.2o (200) which were well matched with the JCPDS card No.36-1451. It confirms that the ZnO nanomaterials possess the hexagonal wurtzite phase with the lattice parameters: a-3.246 and c-5.206 Å. The intensity of (101) diffraction peak is much higher compared to other peaks, indicating the preferential growth direction due to the instability of polar (101) plane (Fig. 18), Moreover, the single peak suggests purity of the grown nanospikes decorated sheets morphology.
Fig.19 (A) shows The J-V characteristics and Fig. (B) shows the UV-Vis spectrum
For the dye desorption:
The J-V characteristics (Fig. 19 A) have been examined to elucidate the performance of the DSSCs fabricated with the photoanodes of PEDOT-ZnO NRs and are measured under a light intensity of 100 mW cm-2 (1.5 AM). DSSC fabricated with the distorted hexagonal ZnO NRs photo anode shows a relatively low solar efficiency of ~1.08%, with a low JSC of ~4.48 mA cm-2, VOC ~0.571 V and FF of ~0.42. However, DSSCs fabricated with the highly ordered tetragonal ZnO NRs photo anode show an appreciably improved overall conversion efficiency of ~3.2% with a high JSC of ~8.7 mA cm-2, VOC of ~0.67 V, and FF of ~0.54. As compared to the distorted hexagonal ZnO NRs photo anode based DSSC, the photovoltaic performance, JSC, VOC and FF are significantly enhanced by ~ 67%, ~48%, ~15% and ~22% respectively. It is seen that the size of the NRs also plays an important role for achieving the high photocurrent density and performance of the device. It is known that the high photovoltaic performance and photocurrent density are related to high light harvesting through the highly uniform and high surface to volume ratio of the photo anode materials at the interface of the sintered nanoparticles and the conducting substrate, depending upon the availability of the active surface for dye adsorption, which perhaps decreases the amount of light absorbed and generates the large number of electrons and holes as against ZnO thin film with smaller particles.
From the UV-Vis spectrum of the dye desorption from dye absorbed Zn NRs photoanodes in NaOH solution, the photoanode of highly ordered tetragonal ZnO NRs attains the higher dye loading than the photoanode of the distorted hexagonal ZnO NRs. Herein, the enhanced photovoltaic performance and JSC are influenced by high orderliness of NRs morphology, high dye loading and improved light harvesting efficiency through the high surface area of the film. However, the unique ordered morphology of the NRs might retard the recombination rate and contribute to longer electron lifetimes, resulting in the increased VOC and FF of device.
CONCLUSION :
Emulsion polymerization has been successfully used as a innovative, cheap and simple synthetic method for PEDOT leading to obtaining a better conductivity product of the order of 150 S/cm which furthers on adding ZnO as a filler material. The polymer PEDOT obtained has got a lamellar or flat sheet like structure which has irregularity in terms of shape or morphology but heating can bring in reasonable regularity in the structure of the polymer and nanocomposite in turn. The properties and structural aspects exhibited by the polymer, PEDOT are in tandem with that reported in the earlier literature82.
Poly (3, 4- ethylene dioxythiophene)/Fe3O4 composites was prepared by in-situ polymerization method. The presence of broad peak of PEDOT at lower angle and sharp peaks of magnetite at higher angles in the XRD pattern confirmed the formation of the PEDOT/Fe3O4 nanocomposites. SEM micrographs showed an increasing trend of the particle size with the increase in Fe3O4 content, which may be due to the effect of agglomeration at higher Fe3O4 content. The particle size of the pure Fe3O4 was found to be 50- 60 nm. It was found that the Fe3O4 nanoparticles were uniformly distributed across the PEDOT matrix at lower loading percentage of the Fe3O4 nanoparticles, whereas agglomeration of the particles was observed at higher loading. The thermo gravimetric analysis exhibited that the thermal stability of the nanocomposite was found to increase with the increase in Fe3O4 content. The magnetic study of the nanocomposites showed that all the samples were highly paramagnetic in nature. The saturation magnetization of the nanocomposites was found to be enhanced with the increase in Fe3O4 content, which indicated that the nanocomposite can be useful for information storage applications. It was found that that for pure magnetite the value of MS was ~ 65 emu/g whereas for the nanocomposite which contains 0.1 g magnetite the value of Ms reduced to~20 emu/g. The reduction in the value of Ms might be due to the nonmagnetic nature of the polymer. However, with further increase in magnetite content the value of Ms increased to ~ 30 emu/g.
SVO-PEDOT nanocomposite clearly shows uniform distribution of SVO in PEDOT due to in-situ polymerization. Structural study also showed the formation of SVO in PEDOT. The SVO nanoparticles so synthesized were found to be distributed uniformly in the PEDOT matrix with the morphology of the nanocomposite particles more of spherical in morphology. The average size of the particles ranges between 5-6 nm.
However, the nanaocomposite PEDOT-ZnO was found to be a better material to be used as a photoanode in DSSC given the characteristic profile of the material.83,84
ACKNOWLEDGEMENT:
Authors are thankful to the Executive Director, Dr. Mangesh T. Karad and Vice Principal, Dr. R.V. Pujeri Vice Principal, MIT College of Engineering, Pune for the financial support and encouragement. Authors are also thankful to the Department of Chemistry, Vidarbha institute of science and humanities, Amravati for allowing us to carry out the experimental work.
REFERENCES:
1. Roncali J. Conjugated poly(thiophenes): Synthesis, Fictionalization and Application // Chem.Rev.-92, 1992, P. 711-738.
2. Andersson M.R., Mammo W., Olinga T., Svensson M., Theander M., Inganas O. Synthesis of Rerioregular Phenyl Substituted Polythiophenes with FeCl3 // Synth.Met.-101, 1999, P. 11-12.
3. McCullough R.D., Williams S.P., Tristram-Magle S., Jayaramann M., Ewbankp.C., Miller L. The First Synthesis and New Properties of Regioregular, Head-To-Tail Coupled Polythiophenes // Synth.Met.-69, 1995, P. 279-282.
4. Niu L., Kvarnström C., Fröberg K., Ivaska A. Electrochemically controlled surface morphology and crystallinity in poly(3,4-ethylenedioxythiophene) films // Synth. Met.-122, 2001, P. 425-429.
5. Lei Y., Oohata H., Kuroda S., Sasaki S., Yamamoto T. Highly Electrically Conductive Poly(3,4-ethylenedioxythiophene) Prepared Via High-Concentration Emulsion Polymerization // Synth. Met.-149, 2005, P. 211-217.
6. L. Groenendaal, F. Jonas, D. Freitag, H. Pielartzik and J. R. Reynolds, Adv. Mater., 12 (2000) 481.
7. G. Heywang and F. Jonas, Adv. Mater., 4 (1992) 116.
8. A. Elschner, S. Kirchmeyer, W. Lvenich, U. Merker and K. Reuter, PEDOT: Principles and application of an intrinsically conductive polymer, Taylor and Francis Group: Boca Raton, (2011).
9. C. J. Brabec, N. S. Sariciftci and J. C. Hummelen, Adv. Funct. Mater., 11 (2001) 15.
10. J. H. Burroughes, D. D. C. Bradley, A. R. Brown, R. N. Marks, K. Mackay, R. H. Friend, P. L. Burns and A. B. Holmes, Nature, 347 (1990) 539.
11. C. G. Wang, J. L. Schindler, C. R. Kannewurf and M. G. Kanatzidis, Chem. Mater., 7 (1995) 58.
12. M. Turbiez, P. Frre, M. Allain, N. Gallego-Planas and J. Roncali, Macromolecules, 38 (2005) 6806.
13. H. J. Spencer, P. J. Skabara, M. Giles, I. McCulloch, S. J. Coles, M. B. Hursthouse, J. Mater. Chem., 15 (2005) 4783.
14. K. Zhang, B. Tieke, J. C. Forgie, F. Vilela, J. A. Parkinson and P. J. Skabara, Polymer, 51 (2010) 6107.
15. C. R. Mason, P. J. Skabara, D. Cupertino, J. Schofield, F. Meghdadi, B. Ebner and N.S. Sariciftci, J. Mater. Chem., 15 (2005) 1446.
16. C. R. Mason, Y. Li, P. O’Brien, N. J. Findlay, P. J. Skabara, J. Org. Chem., 7 (2011) 1722.
17. K. Zhang, B. Tieke, J. C. Forgie, F. Vilela and P. J. Skabara, Macromolecules, 45 (2012) 743.
18. R. Blanco, C. Seoane and J. L. Segura, Tetrahedron Lett., 49 (2008) 2056.
19. C. Pozo-Gonzalo, T. Khan, J. J. W. McDouall, P. J. Skabara, D. M. Roberts, M. E. Light, S. J. Coles, M. B. Hursthouse, H. Neugebauer, A. Cravinod, N. S. Sariciftci, J. Mater. Chem., 12 (2002) 500.
20. H. Pang, P. J. Skabara, D. J. Crouch, W. Duffy, M. Heeney, I. McCulloch, S. J. Coles, P. N. Horton and M. B. Hursthouse, Macromolecules, 40 (2007) 6585. Int. J. Electrochem. Sci., Vol. 9, 2014 4547
21. G. J. McEntee, P. J. Skabara, F. Vilela, S. Tierney, I. D. W. Samuel, S. Gambino, S. J. Coles, M. B. Hursthouse, R. W. Harrington and W. Clegg, Chem. Mater., 22 (2010) 3000.
22. J. Tang, Z. P. Song, N. Shan, L. Z. Zhan, J. Y. Zhang, H. Zhan, Y. H. Zhou, C. M. Zhan, J. Power Sources, 185 (2008) 1434.
23. H. W. Heuer, R. Whermann and S. Kirchmeyer, Adv. Funct. Mater., 12 (2002) 89.
24. S. Kirchmeyer and K. Reuter, J. Mater. Chem., 15 (2005) 2077.
25. J. B. F. N. Engberts and M. J. Blandamer, Chem. Commun., 18 (2001) 1701.
26. U. M. Lindstroem, Chem. Rev., 102 (2002) 2751.
27. R. Breslow, Acc. Chem. Res., 24 (1991) 159.
28. P. A. Grieco, Organic Synthesis in Water, Blacky Academic and Professional: London, (1998).
29. K. Manabe, Y. Mori, T. Wakabayashi, S. Nagayama, S. Kobayashi, J. Am. Chem. Soc., 122 (2000) 7202.
30. Z. Grujic, I. Takakovic and M. Trkovnik, Tetrahedron Lett., 52 (1976) 4823.
31. S. Torri, H. Tanaka, T. Inokuchi, S. Nakane, M. Akada, N. Saito and T. Sirakawa, J. Org. Chem., 47 (1982) 1647.
32. H. Tanaka, Y. Kawakami, K. Goto and M. Kuroboshi, Tetrahedron Lett., 42 (2001) 445.
33. S. Cosnier, Biosens. Bioelectron., 14 (1999) 443.
34. G. G. Wallace, M. Smyth and H. Zhao, Trac-Trend. Anal. Chem., 18 (1999) 245.
35. A. Ryosuke, A. Mahito and F. Toshio, J. Am. Chem. Soc., 127 (2005) 13160.
36. S. S. Zhang, J. Hou, R. Zhang, J. K. Xu, G. M. Nie and S. Z. Pu, Eur. Polym. J., 42 (2006) 149.
37. D. Wojciech, P. Dawid, C-L. Diego, L. K. Alexander, J. S. Peter, Opt. Mater., 33 (2011) 1405.
38. C. Antonio, N. Helmut, P. Andreas, J. S. Peter, J. S. Howard, J. W. M. Joseph, D. Lothar and N. S. Serdar, J. Phys. Chem. B, 110 (2006) 2662.
39. B. Y. Lu, S. M. Zhang, L. Q. Qin, S. Chen, S. J. Zhen and J. K. Xu, Electrochim. Acta, 106 (2013) 201.
40. L. B. Groenendaal, F. Jonas, D. Freitag, H. Pielartzik, and J. R. Reynolds, “Poly (3, 4-ethylenedioxythiophene) and its derivatives: past, present, and future,” Advanced Materials, 2000,12,7, 481–494.
41. V.C. Gonçalves, D.T.Balogh, “Optical chemical sensors using polythiophene derivatives as active layer for detection of volatile organic compounds”, Sensors and Actuators B Chemical, Volume 162, Issue 1, 2012, 307-312.
42. M.Xu, J.Zhang,S.Wang,X.Guo, H.Xia,Y.Wang,S. Zhang,W.Huang, S.Wu, “Gas sensing properties of SnO2 hollow spheres /polythiophene inorganic–organic hybrids” , Sensors and Actuators B: Chemical, Volume 146, Issue 2010, Pages 8-13.
43. Senthilkumar, P.Thenamirtham, R.K.Selvan,“Structural and electrochemical properties of polythiophene”, Applied Surface Science, Volume 257, Issue 21, 15 2011, Pages 9063-9067.
44. M.E.Nicho, H.Hu, C.L.Mata, J.Escalante, “Synthesis of derivatives of polythiophene and their application in an electro chromic device”, Solar Energy Materials and Solar Cells Volume 82, Issues 1–2, 2004, 105-118.
45. S.K. Das, K.Abe, K.Yoshino, Y.Ogomi, S.S. Pandey, S.Hayase,”Controlling the process able ZnO and polythiophene interface for dye-sensitized thin film organic solar cells”, Thin Solid Films, Volume 536, 2013, Pages 302-307.
46. C.H. Lee1,W.Y.Chuang, S.H. Lin, W.J.Wu and C.T. Lin, “APrintable Humidity Sensing Material Based on Conductive Polymer and Nanoparticles” Composites, 2013,05DA08-14.
47. X Guo, J. Jian, L. Lin,H.Zhu and S. Zhu,”O2 plasma-functionalized SWCNTs and PEDOT/PSS composite film assembled by dielectrophoresis for ultrasensitive trimethylamine gas sensor Polythiophene and its derivatives”, Analyst, 2013,138, 5265-5273.
48. J.Jian, X.G.Liwei, L.Qian, C.J.Cheng, J.Li, “Characteristics of dielectrophoretically assembled composite film of oxygen plasma-treated SWCNTs and PEDOT/PSS polymer,”Sensors and Actuators: B 178 (2013) 279– 288.
49. R.S.Diggikar,M.V.Kulkarni,G.M.Kale,B.B. Kale,” Formation of multifunctional nanocomposites with ultrathin layers of polyaniline (PANI) on silver vanadiu oxide (svo) nanospheres by in situ polymerization,”j.mater.chem. a,2013,1, 3992-4001.
50. F.C.Tang, J.Chang, F.C.Wu, H.L.Cheng, S. Lien-C.Hsu, J.S.Chen and W.Y.Chou,“Alignment of poly (3,4-ethylenedioxythiophene) polymer chains in photovoltaic cells by ultraviolet irradiation,”J. Mater. Chem., 2012, 22, 22409-22417.
51. K. D. G. I. Jayawardena, L.J.Rozanski, C.A. Mills, M.J.Beliatis, N.A.Nismy and S. Ravi P. Silva, “Inorganic-in-Organic recent developments and outlook for 4G polymer solar cells,” Nanoscale, 2013, 5, 8411-8427.
52. Liu P.B.,Huang Y.,and Sun X., Liu P.B.,Huang Y.,and Sun X., ACS appl. mater. interfaces,2013, 5 (23),1235.
53. C. Jamie, S.N. Moon, H.S.Creager and S.H.Foulger ,”Electrochemical redox of PEDOTcoated core Shell silica spheres stabilized in a PEG based hydrogel maxtrix: Modulation of the optical properties by doping with various oxidative Mediators,” Int. J. Electro chem. Sci.7 2012 3627-3637.
54. A.Kanwat and J. Jang, “Extremely stable organic photovoltaic incorporated with WOx doped PEDOT: PSS anode buffer layer,” J. Mater. Chem. C, 2014, 2, 901-907.
55. H.Kim, J.Lee, S.Ok and Y.Choe, “Effects of pentacene-doped PEDOT: PSS as a holeconducting layer on the performance characteristics of polymer photovoltaic cells,”Nanoscale research letters 2012,7:5.
56. H.L.Pang,C.T. Huang ,J.H.Chen,et al.,”Preparation of polyaniline-tin dioxide composites and their application in methanol electro-oxidation, “J Solid State Electrochem. 2010, 14,169-174.
57. R.J.Tseng,J.X.Huang, J.Ouyang,et.al.”Polyaniline nanofiber/gold nanoparticle nonvolatile memory,”Nano Lett 2005,5,1077-1080.
58. X.Hana, L.Gaia,H.Jianga,L.Zhaoa,H.Liub, ,W. Zhang,”Core–shell structured Fe3O4/PANI microspheres and their Cr(VI) ion removal properties,”Synthetic Met., 171, 2013, 1- 6.
59. H.Y.Lee,S.P.Rwei,L.Wang,P.H.Chen,”Preparation and characterization of core–shell polyaniline–polystyrene sulfonate@Fe3O4 nanoparticles,” Materials Chemistry and Physics 112 (2008) 805–809.
60. A.Masotti, and A. Caporali, Preparation of Magnetic Carbon Nanotubes (Mag-CNTs) for Biomedical and Biotechnological Applications,”Int. J. Mol. Sci. 2013 December; 14(12): 24619–24642.
61. Wahajuddin and S.Arora “Super paramagnetic iron oxide nanoparticles: magnetic nanoplatforms as drug carriers ,”Int. J. Nanomedicine. 2012; 7: 3445–3471.
62. B. Wenderlinch, Macromolecular Physics, Academic press, New York, 1973.
63. M. Kryezewski, Polym Sci PolymSymp (USA), 1975, 50, 359.
64. C. A. Mead, J. Appl. Phys, 1961, 33, 646.
65. S. C. Chakraborty, N. B. Patil, S. K. Das, S. Basu, Indian J Pure Appl Phys., 1991, 29, 478.
66. P. Kim, N. M. Doss, J. P. Tillotson, P. J. Hotchkiss, M. J. Pan, S. R. Marder, J. Y. Li, J. P. Calame, J. W. Perry, ACS Nano, 2009, 3, 2581.
67. Y. Deng, Y. Zhang, Y. Xiang, G. Wang, H. Xu, J. Mater. Chem., 2009, 19, 2058.
68. X. Y. Huang, L. Y. Xie, P. K. Jiang, G. L. Wang, F. Liu, J. Phys. D: Appl. Phys., 2009, 42, 245407.
69. Z. Li, L. A. Fredin, P. Tewari, S. A. DiBenedetto, M. T. Lanagan, M. A. Ratner T. J. Marks, Chem. Mater., 2010, 22, 5154.
70. J. Li, J. Claude, L. Norena-Franco, S. Seok, Q. Wang, Chem. Mater., 2008, 20, 6304.
71. H. M. Jung, J. H. Kang, S. Y. Yang, J. C. Won, Y. S. Kim, Chem. Mater., 2010, 22, 450.
72. Z. Dang, H. Wang, H. Xu, Appl. Phys. Lett., 2006, 89, 112902.
73. M. N. Tchoul, S. P. Fillery, H. Koerner, L. F. Drummy, F. T. Oyerokun, P. A. Mirau, M. F. Durstock, R. A. Vaia, Chem. Mater., 2010, 22, 1749.
74. T. I. Yang, P. Kofinas, Polymer, 2007, 48, 791.
75. J. Li, S. Seok, B. Chu, F. Dogan, Q. Zhang, Q. Wang, Adv. Mater., 2009, 21, 217.
76. B. Balasubramanian, K. Kraemer, N. Reding, R. Skomski, S. Ducharme and D. Sellmyer, ACS Nano, 2010, 4, 1893.
77. P. Kim, S. Jones, P. Hotchkiss, J. Haddock, B. Kippelen, S. Marder, J. Perry, Adv. Mater., 2007, 19, 1001.
78. S. Ramesh, B. A. Shutzberg, C. Huang, J. Gao, E. P. Giannelis, IEEE Trans. Adv. Packag., 2003, 26, 17.
79. N. Guo, S. DiBenedetto, D. Kwon, L. Wang, M. Russell, M. Lanagan, A. Facchetti, T. Marks, J. Am. Chem. Soc., 2007, 129, 766.
80. N. Guo, S. A. DiBenedetto, P. Tewari, M. T. Lanagan, M. A. Ratner, T. J. Marks, Chem. Mater., 2010, 22, 1567.
81. E. Stefanescu, X. Tan, Z. Lin, N. Bowler, M. Kessler, Polymer, 2010, 51, 5823.
82. M. N. Tchoul, S. P. Fillery, H. Koerner, L. F. Drummy, F. T. Oyerokun, P. A. Mirau, M. F. Durstock, R. A. Vaia, Chem. Mater., 2010, 22, 1749.
83. Shrikaant Kulkarni et al, Synthesis and Characterization of PMMA – CaCO3 nanocomposite, Bionano Frontier, Vol. 8(3), 2015, 84-86,
84. Shrikaant Kulkarni et al, Ultrasound assisted and Characterization of PEDOT – ZnO nanocomposite, International Journal of NanoScience and Nanotechnology. ISSN 0974-3081 6(2), 2015, 101-108.
85. Shrikaant Kulkarni, Sonochemical Synthesis and characterization of PMMA – SiO2 nanocomposite, International Conference on Functional Materials and Microwaves (ICFMM) -2015, BAMU, Aurangabad, December 28-30, 2015...
Received on 23.10.2017 Modified on 12.12.2017
Accepted on 28.12.2017 © AJRC All right reserved
Asian J. Research Chem. 2018; 11(1):91-102.
DOI:10.5958/0974-4150.2018.00020.2